AWS D1.4/D1.4M:2011
Sample Welding Procedure Specification (WPS) Form
Welding Procedure Specification (WPS) No. ______________
Contractor ____________________________________
Authorized by _________________________________
Revision No. ___________________________________
Supporting PQR Identification_____________________
Test Date _____________________________________
WELDING PROCESS:
FCAW-S
FCAW-G
GMAW
SMAW
WELD TYPE:
Groove
Fillet
JOINT TYPE:
Direct Butt
Indirect Butt
T-Joint
Joint(s) Qualified (see Table 6.3) _____________________________________________________________________
Position ________________________
Groove Type____________________________________________________
Root Opening ___________________
Root Face ______________________
Groove Angle _________________
Backing:
Yes
No
Backing Type ___________________________________________________
Backgouging:
Yes
No
Backgouging Method _____________________________________________
TECHNIQUE:
Stringers
Weave
ELECTRICAL CHARACTERISTICS
Current:
AC
DCEP
DCEN
Transfer Mode (GMAW):
Short-circuiting
Globular
Spray
BASE METAL
Material Specification________________________________
Grade _______________________
Welded to:
Material Specification________________________________
Grade _______________________
Maximum Carbon Equivalent _______
Bar size ________________________
Plate Thickness _______________
Coated Bar:
Yes
No
Type of Coating _________________________________________________
FILLER METAL
AWS Specification______________________________
AWS Classification ______________________________
Describe filler metal (if not covered by AWS specifications) _________________________________________________
SHIELDING
Gas:
Single
Mixture
Composition_____________________
Flow rate _____________________
PREHEAT/INTERPASS
Preheat/Interpass Temperature (Min) _______________
Interpass Temperature (Max) ______________________
WELDING PARAMETERS
Current
Travel
Pass
Electrode
Amperage
Volts
Electrical
Speed
Joint
Number(s)
Diameter
Type
Range
Range
Stickout
ipm [mm/min.]
Detail
Manufacturer or Contractor __________________________________________________________________________
Authorized by _______________________________________________________
Date ___________________
Form A-2
56